Lifting

 

 

Description

Shrivelling, swellings, wrinkles or folds of varying severity at the paint surface.

Cause

Non uniform drying within the paint film. This may result from:

  1. Excessive film thickness.
  2. Insufficient drying time between coats, forced drying, non uniform air temperature.
  3. Use of wrong or poor quality thinner.

 

Prevention

  1. Apply paint in thin, even coats.
  2. Allow sufficient drying time between coats, ensure correct, uniform drying temperature.
  3. Use only recommended thinner.

 

Rectification

Allow the film to harden thoroughly. If the defect is slight, flatten, compound and polish the affected area. In severe cases rub down to the substrate and repaint.

 

 

Other Defects:

Πίσω

Cookies

Αυτή η ιστοσελίδα χρησιμοποιεί cookies για να εξασφαλίσει την καλύτερη δυνατή εμπειρία πλοήγησης και να συλλέξει πληροφορίες που είναι σύμφωνες με την πολιτική των cookies. Συνεχίζοντας να χρησιμοποιείτε την ιστοσελίδα μας, δηλώνετε ότι συμφωνείτε να λάβετε τα cookies από την ιστοσελίδα ppgrefinish.com, όπως επεξηγήθηκε στην πολιτική των cookies, εκτός εάν αλλάξετε τις ρυθμίσεις cookies