Crazing

 

 

Description

Appears to the naked eye as a loss of gloss, close examination under low magnification reveals a large number of minute cracks.

Cause

Excessive stresses in the paint film due to:

  1. Inadequate mixing of materials prior to application, insufficient thinning or the wrong grade of thinner.
  2. Excessive film thickness, colour coat applied over inadequately dry or excessively thick under coats.
  3. Incorrect use of additives.

 

Prevention

  1. Always mix paint thoroughly, and use the correct amount of recommended thinner.
  2. Use correct spraying techniques. Apply paint in thin, web films and allow adequate drying time between coats.
  3. Only use approved additives.

 

Rectification

Sand the affected area down to a sound, smooth finish and repaint.

 

 

Other Defects:

Πίσω

Cookies

Αυτή η ιστοσελίδα χρησιμοποιεί cookies για να εξασφαλίσει την καλύτερη δυνατή εμπειρία πλοήγησης και να συλλέξει πληροφορίες που είναι σύμφωνες με την πολιτική των cookies. Συνεχίζοντας να χρησιμοποιείτε την ιστοσελίδα μας, δηλώνετε ότι συμφωνείτε να λάβετε τα cookies από την ιστοσελίδα ppgrefinish.com, όπως επεξηγήθηκε στην πολιτική των cookies, εκτός εάν αλλάξετε τις ρυθμίσεις cookies